Hello Robert, You've gotten some good suggestions already but I am curious about a few things. Why thick gold? (We built such type circuits at Tessera originally to make solid gold ribbon bonds to the IC for the first MicroBGAs) Also what kind of components are to be used? COTS or specialties? Organic or ceramic? Pin counts? Any notions on the operating environment? All that aside, you might take a look at transient liquid phase tin/gold bonding. Good luck Joe --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------