Hi Bob! What specific Pbfree component finish(s) are you dealing with? Dave Hillman Rockwell Collins [log in to unmask] Bob Arciolla <barciolla@ERGPOW ER.COM> To Sent by: TechNet [log in to unmask] <[log in to unmask]> cc Subject 08/10/2005 09:57 [TN] component oxidation AM Please respond to TechNet E-Mail Forum <[log in to unmask]> ; Please respond to Bob Arciolla <barciolla@ERGPOW ER.COM> Good Morning All, We are using lead free components and noticing oxidation. We heard that the oxidation occurs faster on lead free components. Can anyone suggest a method for cleaning these parts. Bob Arciolla Endicott Research Group --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- Quality/Safety Manager --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------