Maybe Napthalene? Moth balls are made from naphthalene, a hydrocarbon derived from coal tar that easily sublimates, or exudes gas acting as a fumigant. Dave S. -----Original Message----- From: Steve Gregory [mailto:[log in to unmask]] Sent: Wednesday, August 24, 2005 1:40 PM To: [log in to unmask] Subject: "Dry" Naphtha Howdy All! I got a call and an email from somebody from one of our other facilities asking about "Dry" Naphtha. I told her I had never heard of it. She said that on the spec sheet for a Dow DC6-1104 RTV, it calls out to mix 80% of Dry Naphtha with it to use for conformal coating I've done a search and can't find anything on Dry Naphtha, I called Tomco-Harwell (where we usually get our chemicals), and called Dow Corning as well, but nobody can tell me what Dry Naptha is, or where to get it. Could it also be known as reagent grade Naphtha? Even better still, has anybody out there worked with Dow DC6-1104 that can help me out about how to apply it as a conformal coating? Kind regards, -Steve Gregory- Senior Process Engineer LaBarge Incorporated Tulsa, Oklahoma (918) 459-2285 (918) 459-2350 FAX __________________________________________________________________ This message may contain information that is privileged and confidential to LaBarge, Inc. It is for use only by the individual or entity named above. If you are not the intended recipient, you may not copy, use or deliver this message to anyone. In such event, you should destroy the message and kindly notify the sender by reply e-mail. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ____________________________________________________________________________ _ Scanned by Sanmina-SCI eShield ____________________________________________________________________________ _ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------