Hi Phil: I believe it was you that originally brought up the hexavalent topic back in July. The correct name is Iridite (14-2 probably being the most famous) which is a trade name originally from Allied-Kelite now owned by MacDermid. The correct call out is chromate conversion coating. Rudy makes a good point, possibly you don't really need a chromate coating. But let me give you the opposite input. If you specify a trivalent coating to replace an existing hexavalent one you could have problems. It depends on what you are using the coating for. If it's for a paint base or a light class three coating you may be OK. If you are using it for corrosion protection in severe environments you could be in trouble. As Denny pointed out discuss the application with the chemical supplier. Then do your testing on your product for qualification and performance. Don't accept what the data sheet says as gospel. Regards Mike Barmuta Staff Engineer Fluke Corp. Everett WA 425-446-6076 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of R Sedlak Sent: Tuesday, August 23, 2005 1:42 PM To: [log in to unmask] Subject: Re: [TN] Specifying RoHS compliant Irradite Phil: Were I in your shoes, I would contact the plater, and find out the name of his vendor for the Iridite.. (I believe that is the spelling?) and contact the vendor, and ask the name(s) of his RoHS compliant coatings... and specify those on your drawings...and get a letter from the chemical vendor assuring you that his products are RoHS compliant. No, you are not alone in this problem... one customer experimented and found that due to other changes they had made in the process, a conversion coating of this type was completely unnecessary...! Rudy Sedlak RD Chemical Company Phil Nutting <[log in to unmask]> wrote: Bev, Gee, that sounds way to easy. Phil -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian Sent: Tuesday, August 23, 2005 3:53 PM To: [log in to unmask] Subject: Re: [TN] Specifying RoHS compliant Irradite Phil, How about you put: "No coating with Cr VI may be used." or some variation thereof on the drawing? Have your plater supply you with his daily/weekly/monthly (pick one) plating bath composition results. Bev RIM -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting Sent: August 23, 2005 3:46 PM To: [log in to unmask] Subject: [TN] Specifying RoHS compliant Irradite This may be outside our groups purview, but I'll ask it anyway. For our aluminum chassis sheet metal we have historically used Yellow Irradiate. The information I'm getting for making this RoHS compliant is to make sure the plating vendor used trivalent chromium rather than hexavalent chromium for either clear or yellow irradiate. It is also my understanding that there are similar "rules" for zinc plating. The real question is, how do I specify this on my assembly drawings and purchase orders? Am I going to get a true RoHS compliant plating? I can't be the only person with this issue! I'm sure I can go into did the plater have a dedicated RoHS plating tank, is he telling me he complies but in reality he just lies? Hey, I'm a cynic. Phil Nutting Design for Manufacturing Engineer Kaiser Systems, Inc. 126 Sohier Road Beverly, MA 01915 voice: 978-922-9300 x1310 fax: 978-922-8374 e-mail: [log in to unmask] www.kaisersystems.com --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- __________________________________________________ Do You Yahoo!? Tired of spam? Yahoo! Mail has the best spam protection around --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- http://mail.yahoo.com --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------