Thanks Dave, I Compared Kester 182 data sheet to J-STD-3 requirements (3.2.2) & it matches exactly. Mark -----Original Message----- From: [log in to unmask] [SMTP:[log in to unmask]] Sent: Wednesday, August 03, 2005 11:15 AM To: [log in to unmask]; [log in to unmask] Cc: [log in to unmask] Subject: Re: [TN] ROL1 flux for solderability testing Hi Mark! Please keep in mind that the JSTD-002 and JSTD-003 requires a specific, defined flux composition recipe and not just any ROL1 flux per JSTD-004. Both specification list the exact flux composition required to be used. Both the JSTD-002 and JSTD-003 committees have requested specific product designation from any/all flux material suppliers to be listed in each of the specifications in section 6 of the next revisions. Dave Hillman Rockwell Collins [log in to unmask] Mark Hargreaves <[log in to unmask]> Sent by: TechNet To <[log in to unmask]> [log in to unmask] cc 08/03/2005 09:51 Subject AM [TN] ROL1 flux for solderability testing Please respond to TechNet E-Mail Forum <[log in to unmask]> ; Please respond to Mark Hargreaves <[log in to unmask]> Hi All, I'm looking for a supplier (in USA) of ROL1 flux (1 gallon or smaller) for low volume solder float solderability testing. Kester 182 looks good (from datasheet) but I can't find a source. Any suggestions? Thanks, Mark Hargreaves EMDS, Inc [log in to unmask] <mailto:[log in to unmask]> --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------