Hi Werner, That is exactly the point I wanted to make. Every time a crack "coalesce" with a void, it would have to re-nucleate again and it's not an easy thing to do. There is one sentence in your e-mail I'd be very cautious about. Some people (and a very limited number of them) they do report the presence of voids at the interface and for some strange reasons call them Kirkendall voids. As far as I know, it have not been any data published, which would show that the presence of those voids were due to the difference in the diffusion rate in between 2 different materials. So, I wouldn't call them Kirkendall voids, just now. :-) Regards, Vladimir Vladimir Igoshev, Ph. D. Senior Materials Researcher Research in Motion 451 Phillip St. Waterloo, ON, N2L 3X2 Voice: (+1) 519-888-7465, ext. 5283 Fax: (+1) 519-886-0863 E-mail: [log in to unmask] -----Original Message----- From: [log in to unmask] [mailto:[log in to unmask]] Sent: Tuesday, July 19, 2005 11:33 AM To: Vladimir Igoshev; [log in to unmask] Subject: Re: [TN] BGA voids Hi Vladimir, You are correct. I have never seen an overstress failure of a solder joint that involved voids in the solder joint bulk volume. I have seen creep-fatigue failures in SJs with voids that did not involve the voids at all, or that went through the voids, but were not caused by them. I have even seen SJs with cracks in them where the cracks stopped at a void. Overstress failures invariably involve the interfaces of solder joints where for a variety of reasons really weak 'links' were created; that includes interfacial failures due to Kirkendall voids. Regards, Werner Engelmaier --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------