________________________________ TechNetters, I have a question that may seem quite elementary to some of you, but I need to ask it anyway. We are evaluating a through hole solder joint to a Class 2 and are experiencing some variation in the circumferential wetting on the secondary side of the PWB. Some of the solder joints are exhibiting 270 degree wetting on the secondary side and also you can see "daylight" through the barrel. According to the standard, 270 degree of solder on secondary side is acceptable, the fact that you can see daylight, though, does concern me. I have examined the IPC-A-610D standard on the various requirements of a solder fillet and the table that states for a Class 2 the solder wetting on the secondary side should be 270 degree wetting to the lead and barrel. I have looked at the vertical fill and it states that 75% is the requirement for the barrel to be filled with solder. My question is with these requirements, if you examine the solder joint and can see "daylight" in the barrel, meaning you can see that there is not a complete fill of solder in the barrel, is this considered a defect? I have also looked at the "pin hole/ blowholes, voids" section and it refers you back to the "criteria table" as to whether you have an acceptable solder joint. Please advise. Thanks. Mary Jane Chism --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------