Glenn: The current electroless Copper bath used to plate on to PCB's is likely to work perfectly on gold, without any changes... many suppliers.. MacDermid, Rohm & Haas, and Electrochemicals.. get them to help you sort it out.. they may well be happy to do samples for you. Rudy Sedlak RD Chemical Company Glenn Pelkey <[log in to unmask]> wrote: Hi folks, Anybody know what the chemical reaction is to plate Copper onto Gold, through the electroless processes (or Galvanic), not electrolytic? To explain further, we know Silver and Nickel can plate on copper through an Electroless or Immersion process. Can that process be reversed where the Copper plates on Silver or Nickel? Or, can a chemistry be developed where the Copper plates on a more noble metal of Gold? Thanks, Glenn --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- __________________________________________________ Do You Yahoo!? Tired of spam? Yahoo! Mail has the best spam protection around --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- http://mail.yahoo.com