If your customer is planning to assemble the boards with lead free solder, then yes, you should drape this project in red velvet. If this just happens to be a RoHS compliant part, but your customer is going to be assembling the boards with Tin Lead solder and keeping their max temp below 220 deg C, then I guess they would be all set. Sounds like the part vendor doesn't really understand what they are doing though. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Dharma Kemp-Bresett Sent: Thursday, June 23, 2005 2:50 PM To: [log in to unmask] Subject: [TN] RE: [TN] RE: [TN] Re: [TN] clarification of tab temp warning vs. lead free temps on comp You are correct. Does this mean that there will have be "special treatment" for this board, if this part is used? I guess I am basically asking if this is a red flag I should be waving at my customer..... Dharma -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Crepeau, Phil (Space Technology) Sent: Thursday, June 23, 2005 2:45 PM To: [log in to unmask] Subject: [TN] RE: [TN] Re: [TN] clarification of tab temp warning vs. lead free temps on comp that may be true, but i believe the concern is that lead free requires higher soldering temperatures. so what to do? maybe that's the question and concern. phil -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Werner Engelmaier Sent: Thursday, June 23, 2005 11:40 AM To: [log in to unmask] Subject: [TN] Re: [TN] clarification of tab temp warning vs. lead free temps on comp Dharma, my dear, hand soldering is the worst possible way to solder when trying to keep the temperature down. Werner --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------