Bob, What ever you do to that floor, DON'T WAX IT! I have an emotional response to you query. In a previous life, we installed an ESD floor and it worked perfectly until a maintenance man one evening waxed it, destroying about 10,000 sq. ft. of ESD floor tiles. Now there may be a floor wax which will not damage the ESD floor tile. I would recommend that you contact the ESD floor tile's manufacturer to determine what materials to use to clean the floor. You will ruin the properties of the floor if you do not follow the maintenance procedures. Hope this helps. Good Luck. Lee Whiteman Senior Manufacturing Engineer American Competitiveness Institute E-Mail: [log in to unmask] Ph: (610) 362-1200 x208 Fax: (610) 362-1290 This message is for informational purposes only and does not supersede, modify, or create any agreements with ACI. Information contained in this message does not bind ACI or its affiliates to any commitment, either express or implied, unless ratified in writing by an authorized representative. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob Arciolla Sent: Tuesday, June 21, 2005 11:43 AM To: [log in to unmask] Subject: [TN] ESD flooring Good Morning All, I have a question regarding ESD flooring. Does flooring tile have to be ESD tile or can you just wax over tile with ESD wax? Thanks, Bob Arciolla Endicott Research Group --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- Quality/Safety Manager --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------