Steve Consider the material of the reel when selecting your bake temperature. Baking at too warm a temperature will make the reel useable. Dave Fish ----- Original Message ----- From: "Stephen Gregory" <[log in to unmask]> To: <[log in to unmask]> Sent: Wednesday, June 15, 2005 9:42 AM Subject: [TN] Baking PLCC-68's... > Just wondering, how many of you have ever baked a > PLCC-68? > > We've been raising the awareness level of our stockroom > people about component moisture sensitivity, and we've > got some PLCC-68's that are on a reel and been sitting on > on our stockroom shelf for longer than 168-hours. > > Well, we got another reel of the same part number (it's an > Intel i960 PLCC-68) that came to us from Avnet in a vacuum > sealed bag with a level-3 MSL label on it. > > I've never baked a PLCC-68...should I bake the reeled parts > that have been sitting on the shelf? > > Kind regards, > > -Steve Gregory- > Senior Process Engineer > LaBarge Incorporated > Tulsa, Oklahoma > (918) 459-2285 > (918) 459-2350 FAX > __________________________________________________________________ > This message may contain information that is privileged and confidential to > LaBarge, Inc. It is for use only by the individual or entity named above. > If you are not the intended recipient, you may not copy, use or deliver > this message to anyone. In such event, you should destroy the message and > kindly notify the sender by reply e-mail. > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 > ----------------------------------------------------- > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------