Hi Ioan, With exposed die and wire bonds, I would say no for production. Maybe they need it for a prototype... Risk are, flux contamination, solder balls, handling damage. The reflow temperature itself is not a problem, just everything that goes with it. Glenn -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea, Ioan Sent: Thursday, June 30, 2005 7:49 AM To: [log in to unmask] Subject: [TN] Is wire bonding reflowable? Hi Technetters, a customer of ours is wondering if a module they are ordering will be OK to solder in regular (SnPb for now) reflow. The module has an exposed die, no encapsulation, wire bonded to gold pads on an FR4 substrate. For me, since regular ICs can be reflowed with no issue, this module should not present any hickup. My exposure to wire bonding is zero, so I take this issue with you. Can this question be answered as is, or would you need more details? Thanks, Ioan --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------