Hi Richard! I asked that question of a former applications engineer (now sales engineer) of Fein Focus when she was here giving me a presentation on their Tiger series system Tuesday. I asked that question because their system can put out 160 kV at 1 mA. I was told the only component that she has heard of possibly becoming damaged was memory. She wasn't able to give me a specific level, but she did say that it would need to be directed at the component for an extended period of time. She added that she hasn't heard of a Fein Focus system ever damaging components. Kind regards, -Steve Gregory- Senior Process Engineer LaBarge Incorporated Tulsa, Oklahoma (918) 459-2285 (918) 459-2350 FAX |---------+----------------------------> | | "Stadem, Richard"| | | <Richard.Stadem@G| | | D-AIS.COM> | | | Sent by: TechNet | | | <[log in to unmask]>| | | | | | | | | 06/16/2005 08:47 | | | AM | | | Please respond to| | | TechNet E-Mail | | | Forum; Please | | | respond to | | | "Stadem, Richard"| | | | |---------+----------------------------> >--------------------------------------------------------------------------------------------------------------| | | | To: [log in to unmask] | | cc: | | Subject: [TN] X-ray radiation limits | >--------------------------------------------------------------------------------------------------------------| Does anyone have information on the X-ray radiation levels that can potentially harm electronic components? I am looking for standards (IPC or otherwise) that detail or recommend dosage limits for various component package types and sizes. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- __________________________________________________________________ This message may contain information that is privileged and confidential to LaBarge, Inc. It is for use only by the individual or entity named above. If you are not the intended recipient, you may not copy, use or deliver this message to anyone. In such event, you should destroy the message and kindly notify the sender by reply e-mail. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------