Ioan, I'll add a few comments to the thread. At 06:38 AM 6/14/2005, you wrote: >1. The ceramic caps will be more prone to internal cracks when on >lead-free. To prevent that it is necessary to eliminate the fillets and >make the joints thicker. I've been through major fighting here to get the >designers stick to IPC-7531, now I have to make them change the CCs... >Well, that's my problem. On the other hand, besides overprinting, are >there any other solutions to increase the height of the solder joint (I >assume applications where stencils thicker than 6 mils are not an option) Perhaps reduce solder fillet size and use somewhat smaller pads. Large pads and fillets have been a problem in the past and will only become more troublesome in the future. >2. Recently Ingemar made a statement on the tantalum caps, that they >should be a stay-away. Why? Tantalum capacitors have dielectric flaws when shipped directly from the factory. They are made from clean dirt but when dealing with <100 nM thick dielectric layers any contamination like a small bit of nickel results in very thin dielectric layers resulting in localized leakage current and depending on current density joule heating. Unfortunately the dielectric has a couple of stable phases, amphorous and crystalline, the amphorus being a good dielectric and crystalline an excellent current conductor. That is why tantalum caps were first developed with MnO2 cathodes, as flaws heat up due to joule heating of the cathode converts to an insulator as oxygen is robbed from the cathode layer in effect scabbing over. Polymer cathode parts do not scab and are limited to low voltage parts in part of no self heal mechanism being present other than vaporization of the polymer. Tantalum pent oxide also has another interesting characteristic, it is electrostrictive or grows in the direction of the applied field and this movement coupled with impurities like nickel or other non valve metals can lead to "inrush" current failures. It is really a dV/dt and not a current phenomena. Now that I am back consulting I just love lead free soldering, ceramic and tantalum caps John Maxwell --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------