You can get all the info you want on the NEMI website. There is currently a lot of IC industry interest in pushing the matte tin thickness spec up to 10 micrometers from the current typical 7-8 micrometers due to the belief that the thicker material will provide a better whisker performance, but little substantiating data is available. Best regards, Leo Director of Applications Engineering ASAT, Inc. 3755 Capital of Texas Highway, Suite 100 Austin, Texas 78704 ph 512-383-4593 fx 512-383-1590 [log in to unmask] www.asat.com The information contained in this electronic message is CUSTOMER/SUPPLIER PRIVILEGED AND CONFIDENTIAL INFORMATION intended only for the use of the individual or entity named above. If the reader of this message is not the intended recipient, you are hereby notified that any dissemination, distribution and copying of this communication is strictly prohibited. If you have received this communication in error, please immediately notify the sender by electronic mail. Thank you. -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Jana Carraway Sent: Friday, June 10, 2005 10:08 AM To: [log in to unmask] Subject: [TN] Matte Tin specification question Good Morning TechNet, Could someone point me in the direction of a specification for required plating thickness of matte tin? Or if someone knows the industry recommended thickness, please pass that along. The application would be for component leads, not final finish on the pc board. Thank you for the help, Jana Carraway Jana Carraway MSEI - Advanced Technology Group 6024 S.W. Jean Road Lake Oswego, OR 97035 503.697.5291, ext 1180 email: [log in to unmask] --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------