http://www.enthone-omi.com/pwb/index.aspx?Detail=pwb_entek-plus.ascx http://www.enthone-omi.com/pwb/index.aspx?Detail=pwb_entek-plus-ht.ascx These are the ones I am acquainted with above.. Bill Brooks - KG6VVP PCB Design Engineer, C.I.D.+, C.I.I. Tel: (760)597-1500 Ext 3772 Fax: (760)597-1510 Datron World Communications, Inc. _______________________________________ San Diego Chapter of the IPC Designers Council Communications Officer, Web Manager http://dcchapters.ipc.org/SanDiego/ http://pcbwizards.com -----Original Message----- From: Bev Christian [mailto:[log in to unmask]] Sent: Thursday, June 16, 2005 5:36 AM To: [log in to unmask] Subject: [TN] Current Suppliers of OSP Good morning! Who are the CURRENT suppliers of OSP around the world? Google is useless. BevRIM --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------