An excellent article on the P content and its effects on solderability is in the September 2002 copy of Global SMT and Packaging. It is titled "The Black Pad Failure Mechanism, From Beginning to End". It was written by a number of engineers with Cookson/Alpha Metals. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis Sent: Friday, May 27, 2005 9:37 AM To: [log in to unmask] Subject: Re: [TN] Solderablity of ElectrolessNickel (B. Dunn, Metallurgical Assessment of Spacecraft Parts, Materials > and Processes) My God, I thought I was the only one with that book on my shelves!!! Brian --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------