I would propose that, in a microsection view, the distance from drilled edge to opposing pad edge does not exceed the pad size as measured at the pad base. So a .028" pad being drilled should never yield a total measurement beyond .028" or the pad has breakout. Jeffrey Bush Director, Quality Assurance and Technical Support VERMONT CIRCUITS INCORPORATED 76 Technology Drive - POB 1890 Brattleboro, Vermont 05302 Voice: 802.257.4571.21 Fax: 802.257.0011 http://www.vtcircuits.com -----Original Message----- From: Susan Mansilla [mailto:[log in to unmask]] Sent: Friday, May 27, 2005 10:02 AM To: [log in to unmask] Subject: [TN] Tangency Definition This is probably a good topic for Friday.... We, the industry, need a definition of the word tangency as it applies to a registration condition noted in a microsection. Do any of you have something that could be proposed to the T-50 group? Susan Mansilla Robisan Laboratory --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------