Bright Watts NI - or a hard gold plate over low stress NI. Jeffrey Bush Director, Quality Assurance and Technical Support VERMONT CIRCUITS INCORPORATED 76 Technology Drive - POB 1890 Brattleboro, Vermont 05302 Voice: 802.257.4571.21 Fax: 802.257.0011 http://www.vtcircuits.com -----Original Message----- From: Roger M Unwin [mailto:[log in to unmask]] Sent: Monday, May 23, 2005 3:06 PM To: [log in to unmask] Subject: [TN] PCB Commutator Hi Technetters, Any suggestions for a good hard wearing finish that would extend the life of 3oz copper tracks being used as a sort of commutator. Am told that first prototypes were made with chemical (Electroless?) gold over nickel. Some lasted well, others not so well. Brushes are metal, sorry don't know the composition. Approx. 5 amps current passes through connections. Thank you for your assistance -- Roger M Unwin P+M Services (R) Ltd Tel : 01706 815212 Fax : 01706 818636 Http://www.p-m-services.co.uk --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------