What is the standard thickness for electrolytic gold plate on BGA pads? My customer's print is calling out .000030" minimum per MIL-G-45204 type C class 1 over nickel plate .000150" per QQ-N-290 class 1 type 7. I have misplaced my mil specs and do not remember the classes and types. Can someone translate please? I am thinking that is too much gold for surface mount soldering. Wouldn't the joint be dull and brittle? Judy -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of R Sedlak Sent: Tuesday, May 03, 2005 5:39 PM To: [log in to unmask] Subject: Re: [TN] minimum nickel thickness` Phil: Are you talking electroless or electrolytic Nickel? I believe electroless to be MUCH more robust, and less pore prone. I would want 50% more electrolytic than electroless for the same protection, but even this 50% factor can vary dramatically depending on plating rate. Other question is this for simply surface mount, or, what other places will it be done on the PCB? Will the board have tabs, and be inserted and removed frequently? So, as in many situations, the best answer probably is, "It depends". Rudy Sedlak RD Chemical Company "Crepeau, Phil (Space Technology)" <[log in to unmask]> wrote: hi, forgetting about ipc spec requirements, what is the minimum nickel plating thickness over copper on a printed wiring board that you would feel comfortable with as a barrier against copper migration. thanks, phil --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- __________________________________________________ Do You Yahoo!? Tired of spam? Yahoo! Mail has the best spam protection around --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- http://mail.yahoo.com --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------