Pete, I would think the effect would be dependent on the trace width or amount of copper that supports the current. This web site might help with the calculation. http://www.geocities.com/CapeCanaveral/Lab/9643/TraceWidth.htm good luck. Dave Pete menuez wrote: > All: > > We had an assembly in test and one of the technicians accidently probed a > pad and shorted the probe to ground. This drew about 1.6 amps > (calculated) > for about 100 miliseconds. > > Is there a chart, guideline, calculation or something that will tell > me what > damage would occur to the internal trace/laminate with such an event. > > Thanks in advance, > > Pete > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: > http://listserv.ipc.org/archives > Please visit IPC web site > http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional > information, or contact Keach Sasamori at [log in to unmask] or > 847-615-7100 ext.2815 > ----------------------------------------------------- > > -- Dave Seymour, CID+ Catapult Communications Inc. 800 Perimeter Park Dr, Suite A Morrisville, NC 27560 Direct: (919)653-4249 Main: (919)653-4180 Fax: (919)653-4297 [log in to unmask] --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------