Without further requirement description, like temperature extremes, Acrylic is the more producible choice for reason of easy reworkability and clean-up. We use it on hi-rel space products. Parylene is the best if high voltage (500v) and environment demand it but on the bottom of the desirability list. You will end up cursing it unless there is no way the assy will ever need to be reworked. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Barbara Burcham Sent: Monday, May 16, 2005 5:56 PM To: [log in to unmask] Subject: [TN] Conformal Coating of Assembled Boards Well, my company now has an application requiring conformal coating on some small assembled boards. We need to mask off 3 connectors and coat everything else. I have some information on a product called Parylene applied by Parylene Coating Services, Inc. in Katy, Texas. We did a small lot with a simple spray-on process, but that is not the way to do production runs, of course. What would you recommend? Thanks, Barbara Barbara J. Burcham, C.I.D. Fairfield Industries, Inc 281-275-7687 [log in to unmask] --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------