Greg, Back when we were in the wave solder business we had a solder pot start leaking. It was still under warranty so the manufacturer came to our facility and emptied the pot. I couldn't believe it but he used a ladle and "Paper" soup bowls. They were the thick ones especially designed for soup and not the plastic foam ones but paper. He only ran the pot temperature up to a little above molten. Low and behold they worked great! He filled them about 2/3's full and they set up into really nice ingots that we could reuse. Might be worth a try. KennyB TechNet: We are going to drain and clean a wave solder pot in preparation for conversion to lead-free solder. We have not completely purged a wave solder pot in some time, and the people in the know have moved on. Does anyone have "best practices" recommendations for draining and handling the solder (other than BE VERY CAREFUL ! ) ? Greg Anderson GE Fanuc Automation Charlottesville, VA --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------