If the design is SMOBC this process is in violation. We have seen specific references to not put tin of silver under the soldermask. Jeffrey Bush Director, Quality Assurance and Technical Support VERMONT CIRCUITS INCORPORATED 76 Technology Drive - POB 1890 Brattleboro, Vermont 05302 Voice: 802.257.4571.21 Fax: 802.257.0011 http://www.vtcircuits.com -----Original Message----- From: Stephen M. Vargas [mailto:[log in to unmask]] Sent: Friday, April 01, 2005 8:42 AM To: [log in to unmask] Subject: [TN] Immersion Silver Good Day All: A question arose at our factory regarding immersion silver surface finish. We recieved boards where the solder masking was applied after the immersion silver was applied to the PWB. Are there potential solder mask adhesion issues with this? Should the solder mask be applied prior to adding the surface finish? Any insight would be appreciated. Thanks. Regards, Steve Vargas --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------