Are you looking for information on how to make the section or are you looking for information on what attributes to evaluate on the drilled hole wall. One important thing is to have a light electroless deposit on the hole wall before sectioning so you can easily see the topography of the hole wall - otherwise it is sometimes difficult to tell where the mounting resin begins and the laminate ends. Susan Mansilla Technical Director Robisan Laboratory, Inc 6502 E. 21st Street Indianapolis, IN 46219 317-353-6249 317-917-2379 fax www.robisan.com -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Parial Swati Sent: Tuesday, April 12, 2005 12:51 AM To: [log in to unmask] Subject: [TN] Microsection for checking hole quality Dear friends, Are there any guidelines available regarding the microsections done for checking the drill hole quality ? Any web sites or ipc document reference will also be very helpful. Thanks. Warm regards, Swati Parial Scan by AT&S virus protection --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------