Paul, we run SN96 here A LOT and it is, by design, 96.5/3.5. The SAC alloy is the same, but with .5 percent copper taking away from the silver side. Jason Gregory Manufacturing Engineer Innova Electronics (281)653-5593 (281)653-5594 fax (281)212-0844 cell [log in to unmask] -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Stolar, Paul W Sent: Monday, April 11, 2005 9:08 AM To: [log in to unmask] Subject: [TN] Pb-Free Does anyone think that 3.5% Pb in a SN96AG4 (aka Pb-free) is abnormal? I think it is, but I have doubters here. This was measured by EDX. Does anyone have any evidence what this does to reliability? Specifically mechanical cycling. Paul Stolar Materials/Reliability Engineer Manufacturing Reliability Lead Engineer Baker Atlas 713-625-5376 --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------