How long does it need to adhere? What temperature range will this be used in? If there is much of a range of temperatures, the differential expansion might cause any adhesive to fail. You might have better luck with a thicker adhesive film such as 3M VHB, as is used to adhere body side moldings to cars. I don't know how well this would adhere to Delrin, though. The thicker film (usually a foam-type material) absorbs much of the differential expansion, allowing both materials to remain bonded over wider temperature ranges. Dave Roach Trane GCC 4833 White Bear Parkway St. Paul, Minnesota 55110 651-407-4294 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Chad Haima Sent: Tuesday, March 01, 2005 11:53 AM To: [log in to unmask] Subject: [TN] Help!! Anybody have some recommendations for glueing delrin and stainless steel together. We're going through loctite and are getting nowhere. Any help is much appreciated. Thanks, Chad Haima Pentagon EMS Ph: 503-924-2747 Fx: 503-924-2744 [log in to unmask] www.pentagon-ems.com --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------