Our coating process spec says coating application must be within 3 days if stored in dry, dust-free environment. In reality, the assemblies get coated within 8 hours of vacuum oven removal. > Rainer G. Blomberg > Honeywell -Space Systems Clearwater > Staff Production Engineer (727) 539-5534 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Dehoyos, Ramon Sent: Thursday, March 03, 2005 10:12 AM To: [log in to unmask] Subject: [TN] Cleaning Window Question to the forum: What is the time window between cleaning/bake dry and Conformal Coating? I hear from 32 hours to indefinite. What is your experience? Best Regards, Ramon --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------