It depends.... What results are you trying to 'not affect'? Nickel is lossy at RF frequencies.. The higher the freq. and longer the transmission line the worse the effect gets if I remember correctly from my Microwave days... Does it change the impedance of the line... probably not. Impedance is a result of the relationship between the dk of the material, distance of the conductor from it's return path or ground plane and the width of the transmission line... in a microstrip arrangement. I don't believe the thickness of the plating is a large enough influence on the line to change the impedance by any measurable amount. But lossy RF might be a reason to choose a different surface finish that doesn't contain nickel. Especially if you are dealing with very low voltage signals... It's kind of like a trickling stream running along a nice solid rock bed and then suddenly hitting a huge sand bar... where the water slows and sinks into the sand... disappearing from view completely... You don't want nickel plating on high frequency boards. If it's not that sort of an application, then you most likely will not have a problem. Best regards, Bill Brooks - KG6VVP PCB Design Engineer , C.I.D.+, C.I.I. Tel: (760)597-1500 Ext 3772 Fax: (760)597-1510 e-mail:[log in to unmask] http://www.dtwc.com http://pcbwizards.com -----Original Message----- From: Steve [mailto:[log in to unmask]] Sent: Wednesday, March 16, 2005 4:00 PM To: [log in to unmask] Subject: [TN] Immersion gold Good afternoon, A question for the guru's. If I do immersion gold/electroless nickel on top of an impedance line will it affect the result. Thanks in advance. Steve Kelly Sent via BlackBerry Steve Kelly PFC Flexible Circuits Limited --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------