Delrin is a difficult plastic to get anything to adhere to, as it is a "waxy" plastic. You might have some success with a two-part epoxy. I would recommend scuffing the surface of the Delrin before gluing. Dave Roach Trane GCC 4833 White Bear Parkway St. Paul, Minnesota 55110 651-407-4294 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Chad Haima Sent: Tuesday, March 01, 2005 11:53 AM To: [log in to unmask] Subject: [TN] Help!! Anybody have some recommendations for glueing delrin and stainless steel together. We're going through loctite and are getting nowhere. Any help is much appreciated. Thanks, Chad Haima Pentagon EMS Ph: 503-924-2747 Fx: 503-924-2744 [log in to unmask] www.pentagon-ems.com --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------