Calgary? If you want extreme cold in a fairly major Canadian city, I wouldn't choose Calgary (wimps...heehee). Consider Edmonton, or maybe better yet, Winnipeg. Sorry, I should have waited for Friday with this post. -----Original Message----- From: Mcmaster, Michael [mailto:[log in to unmask]] Sent: February 3, 2005 10:58 AM To: [log in to unmask] Subject: Re: [TN] Behavior of Via's in low temperature cycling Wouldn't a city such as Minneapolis or Calgary be a more appropriate location for this conference? You know somewhere where they have electrical outlets in the parking lots and plugs hanging out of the grills of the cars. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo Sent: Thursday, February 03, 2005 6:45 AM To: [log in to unmask] Subject: Re: [TN] Behavior of Via's in low temperature cycling more commercialism: There is still time to register and attend the IMAPS Advanced Technology Workshop on Reliability of Advanced Electronic Packages and Devices in Extreme Cold Environments. February 21 - 23, 2005 Hilton Hotel Pasadena, California Ph: 1-800-HILTONS or 626-577-1000 Please visit http://www.imaps.org/extremecold for the complete program and to register to attend -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Leo Higgins Sent: Wednesday, February 02, 2005 8:20 PM To: [log in to unmask] Subject: Re: [TN] Behavior of Via's in low temperature cycling ....commercialism? Best regards, Leo Director of Applications Engineering ASAT, Inc. 3755 Capital of Texas Highway, Suite 100 Austin, Texas 78704 ph 512-383-4593 fx 512-383-1590 [log in to unmask] www.asat.com The information contained in this electronic message is CUSTOMER/SUPPLIER PRIVILEGED AND CONFIDENTIAL INFORMATION intended only for the use of the individual or entity named above. If the reader of this message is not the intended recipient, you are hereby notified that any dissemination, distribution and copying of this communication is strictly prohibited. If you have received this communication in error, please immediately notify the sender by electronic mail. Thank you. -----Original Message----- From: Werner Engelmaier [mailto:[log in to unmask]] Sent: Tuesday, February 01, 2005 7:34 PM To: [log in to unmask] Subject: Re: [TN] Behavior of Via's in low temperature cycling Hi Rich, I give a whole workshop on this. go to my website for info. Regards, Werner Engelmaier Engelmaier Associates, L.C. Electronic Packaging, Interconnection and Reliability Consulting 7 Jasmine Run Ormond Beach, FL 32174 USA Phone: 386-437-8747, Fax: 386-437-8737, Cell: 386-316-5904 E-mail: [log in to unmask], Website: www.engelmaier.com --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------