Solder plated copper core balls are available with sizes from about 0.25 - 0.5mm dia. Not sure what types of solder plating finishes are available, but suspect PbFree materials maybe available. BGA mfg with such balls likely to be a non-standard product. Senju-Comtek is one source for the balls ( http://www.senjucomtek.com ). Best regards, Leo Director of Applications Engineering ASAT, Inc. 3755 Capital of Texas Highway, Suite 100 Austin, Texas 78704 ph 512-383-4593 fx 512-383-1590 [log in to unmask] www.asat.com The information contained in this electronic message is CUSTOMER/SUPPLIER PRIVILEGED AND CONFIDENTIAL INFORMATION intended only for the use of the individual or entity named above. If the reader of this message is not the intended recipient, you are hereby notified that any dissemination, distribution and copying of this communication is strictly prohibited. If you have received this communication in error, please immediately notify the sender by electronic mail. Thank you. -----Original Message----- From: Michael Forrester [mailto:[log in to unmask]] Sent: Thursday, February 24, 2005 8:29 AM To: [log in to unmask] Subject: [TN] Fixed Z-Axis Lead Free BGA We currently have a number of custom BGAs using high lead balls to maintain a fixed Z-axis height. We are trying to move them to a lead free. What alternatives are out there? I have read about a polymer core ball but am concerned about the current carrying capability of such a ball, our devices are typically high power. Any information would be greatly appreciated. Thank you. Best Regards, Mike Forrester --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------