The relative conductivity of Copper is about twice that of aluminum. Regards, Ramon -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Denis Lefebvre Sent: Thursday, January 13, 2005 2:25 PM To: [log in to unmask] Subject: Re: [TN] Aluminum substrates... any issues? I've heard of "copper core" boards before, but not aluminum. I suppose it would preferable with respect to the fact that aluminum is a better conductor than copper. -----Original Message----- From: Brooks,Bill [mailto:[log in to unmask]] Sent: Thursday, January 13, 2005 11:08 AM To: [log in to unmask] Subject: [TN] Aluminum substrates... any issues? I ran across this supplier of aluminum boards and was interested if any of you have dealt with this type of thing before? I have seen metal core boards made with alumina and bonded with the fiberglass/epoxy for heat sinking needs but this looks like a different process. Possibly less expensive... ??? http://www.irctt.com/pdf_files/thickfilm_aluminum.pdf Any comments on it are appreciated. Best regards, Bill Brooks - KG6VVP PCB Design Engineer , C.I.D.+, C.I.I. Tel: (760)597-1500 Ext 3772 Fax: (760)597-1510 e-mail:[log in to unmask] http://www.dtwc.com http://pcbwizards.com --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------