Downloaded it from Humiseal this P.M. (revised 11-10-13?) Store at room temperature, away from direct sunlight...etc. It also says Humiseal products may be stored at 0-100F. It does recommend allowing it to equilibriate at 65-90F for 24 hours. I'll send a copy to your e-mail. Mike Rob Carrillo <[log in to unmask] To: [log in to unmask] OM> cc: Sent by: TechNet Subject: Re: [TN] HumiSeal 1B73 <[log in to unmask]> 01/21/2005 03:43 PM Please respond to TechNet E-Mail Forum; Please respond to Rob Carrillo The latest datasheet, 1755-EFF-15/11-99 from 1999 only states 6 months at 10 degrees C. Is this the same datasheet? Robert Carrillo Quality Manager North Atlantic Industries -----Original Message----- From: [log in to unmask] [mailto:[log in to unmask]] Sent: Friday, January 21, 2005 4:35 PM To: TechNet E-Mail Forum; Rob Carrillo Subject: Re: [TN] HumiSeal 1B73 12 mo. at room temperature, according to the datasheet. Mike Sewell Production Manager LaBarge inc Rob Carrillo <[log in to unmask] To: [log in to unmask] OM> cc: Sent by: TechNet Subject: Re: [TN] HumiSeal 1B73 <[log in to unmask]> 01/21/2005 03:28 PM Please respond to TechNet E-Mail Forum; Please respond to Rob Carrillo Is storing at 20-25deg.C in violation of the manufacturer's specification? What is the shelf life at 20-25deg.C? Rob Carrillo Quality Manager North Atlantic Industries Bohemia, Long Island, NY -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Leigh Jansen Sent: Wednesday, January 19, 2005 11:58 AM To: [log in to unmask] Subject: Re: [TN] HumiSeal 1B73 Hello Rob, I would recommend storing such a solvent based Acrylic conformal coating between 20-25deg.C ideally, thereby having it ready to use in your application. Any colder and you may have to wait a long time before it is at operating/application temperature, particularly in 25litre drums. Any hotter and you may suffer more rapid, undesirable evaporative losses of the solvent, also causing higher odour levels. Storing at this temperature means the viscosity is then controlled ready for use straight out of the drum, as supplied. As you may know, a change of 5cps in viscosity can cause immense problems in selective coating applications. If odour and flammability limits are your reasons for cold storage, then maybe you could address this by looking at a water based Acrylic ? Hope this helps, Leigh Jansen Technical Support Manager NEW - HumiSeal 1H2O BoV Aerosol - NEW [log in to unmask] Concoat Limited - Engineering Reliability in Electronics www.concoat.co.uk 9-11 Fleet Road,Fleet, Hampshire GU51 3QF Tel: +44 (0)1252 813706 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Dehoyos, Ramon Sent: 19 January 2005 15:25 To: [log in to unmask] Subject: Re: [TN] HumiSeal 1B73 Hi Rob: There are plenty of inexpensive industrial refrigerators Hook up a chart recorder to it and keep it at the temp you want. We use them for some glues. Regards, Ramon -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Rob Carrillo Sent: Wednesday, January 19, 2005 9:25 AM To: [log in to unmask] Subject: [TN] HumiSeal 1B73 I am looking for some recommendations on how to store HumiSeal 1B73 under the revised storage temp. of +10°C. We purchase the item in 5 gallon drums and keep it at point of use. Refrigeration in the work cell may prove difficult. Any suggestions would be appreciated unless we repackage into smaller containers. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- __________________________________________________________________ This message may contain information that is privileged and confidential to LaBarge, Inc. It is for use only by the individual or entity named above. If you are not the intended recipient, you may not copy, use or deliver this message to anyone. In such event, you should destroy the message and kindly notify the sender by reply e-mail. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- __________________________________________________________________ This message may contain information that is privileged and confidential to LaBarge, Inc. It is for use only by the individual or entity named above. If you are not the intended recipient, you may not copy, use or deliver this message to anyone. In such event, you should destroy the message and kindly notify the sender by reply e-mail. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------