I will use Doug Paul's "famous" quip - It depends. In an "as polished" mount - you will 9 times out of 100 see no line of demarcation between the end of the inner layer and the plated hole wall copper. There are a couple of ways that you will see a line in this condition 1) when you have gross separations 2) when you have a very thick electroless deposit. Now you may or may not see a line in the as polished condition if you have separation. That will depend on amount of separation and smearing of the polish on the surface of the mount. This is similar to the fact that you will not see cracking in copper in the as polished condition. After the metalurgical microetch (50/50 ammonium hydroxide/hydrogen peroxide) you will have a line if the boards were produced with electroless copper as the hole metalization. If "direct metalization" is used, you may or may not have a line. Let me know if you have further questions. Susan Mansilla Technical Director Robisan Lab 317-353-6249 www.robisan.com --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------