This is probably a normal (acceptable) condition. As to why earlier sections showed no demarcation line and this one did may be the amount of etch used to expose the demarcation line. Some shops like to etch as little as possible - to just expose the demarcation - so they don't discolor the electroless. Electroless copper, if this is what was used, may turn black making the connection look separated. It is always a good idea to review the sections prior to etch to see if there is any separation. Some one may want to challenge me on this but generally if you have post separation you will see it before etch. (An exception to this is if the cross section grinding smeared copper across the interface hiding the separation.) pete >From: "Finks, Tim (Healdsburg)" <[log in to unmask]> >Reply-To: TechNet E-Mail Forum <[log in to unmask]>, "Finks, Tim >(Healdsburg)" <[log in to unmask]> >To: [log in to unmask] >Subject: [TN] Inner layer to barrel connection quality >Date: Mon, 10 Jan 2005 14:15:29 -0800 > >I have PTH cross-section images which show a visible interface between >inner >layer foils and the PTH plating. Earlier, similar, board cross-sections >show >no discernable interface - the inner layer foil and the barrel plating >appear to be integral. > >What should I see when I have an acceptable PWB? > > > >Regards, > >Tim Finks > >--------------------------------------------------- >Technet Mail List provided as a service by IPC using LISTSERV 1.8e >To unsubscribe, send a message to [log in to unmask] with following text in >the BODY (NOT the subject field): SIGNOFF Technet >To temporarily halt or (re-start) delivery of Technet send e-mail to >[log in to unmask]: SET Technet NOMAIL or (MAIL) >To receive ONE mailing per day of all the posts: send e-mail to >[log in to unmask]: SET Technet Digest >Search the archives of previous posts at: http://listserv.ipc.org/archives >Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 >for additional information, or contact Keach Sasamori at [log in to unmask] or >847-615-7100 ext.2815 >----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------