Kaye: The likliest scenario is this.. the VCI you refer too is likely a benzotriazole based chemistry, that is the most common. It is also probable that your IAg contains benzotriazole already, this is co-deposited with the Silver, in most systems. So the most probable situation is that you would be applying more of something that is already there... The implications of this are that the upside benefits are likely low, and the downside potential problems are also low... Without knowing specifics, that is probably the best guess. Rudy Sedlak RD Chemical Company Kaye Clayo <[log in to unmask]> wrote: Hi Technet, Does anyone have any experience using vapor corrosion inhibitors (VCI's), and if so, would this be suitable (or even necessary) to use to store raw immersion silver finished printed circuit boards or partially assembled IAg boards to extend the shelf life of the finish? It is my understanding that VCI's "work" by seeding the air surrounding the metal object and depositing (electrons?) on the surface which protects the finish from corroding (tarnishing), and that they can have a variety of proprietary chemical compounds to do this. I am concerned whether or not the VCI's can affect the solderability of the IAg surface finish, and also the personal health risks involved (if any). There is a paper called silver saver paper that has the VCI chemical sprayed onto it. I am questioning if this is OK to use to slip sheet IAg boards. There are also VCI plastic bags. I guess my ultimate question would be how to store the IAg boards after the package is opened and before final assembly (what kind of bags or boxes or such and whether they should be vacuum packed). Thank you in advance for your thoughts. Kaye Clayo CONFIDENTIALITY NOTE: This message is intended only for the use of the individual or entity to which it is addressed and may contain information that is privileged, confidential, and exempt from disclosure under applicable law. If the reader of this notice is not the intended recipient, you are hereby notified that any dissemination, distribution or copying of this communication is strictly prohibited. If you have received this communication in error, please notify the sender immediately. _____________________________________________________________________________ Scanned by IBM Email Security Management Services powered by MessageLabs. For more information please visit http://www.ers.ibm.com _____________________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- __________________________________________________ Do You Yahoo!? Tired of spam? Yahoo! Mail has the best spam protection around --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- http://mail.yahoo.com