Actually it is not all that unique. We have completed our material and process qualification for lead-free reflow soldering and have developed a lead-free reflow soldering process that does not include Nitrogen. It will be going into Hi-Volume production in April 2005. Best Regards, Mark Krmpotich DFx Engineer World Wide Operations Technology Scientific Atlanta *[log in to unmask] http://www.scientificatlanta.com/ -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Ingemar Hernefjord (KC/EMW) Sent: Thursday, January 13, 2005 4:17 AM To: [log in to unmask] Subject: Re: [TN] Antw: [TN] Must we applied N2 to reflow when using Pb-fr ee solder paste? the Swiss are unique.... Ingemar -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Le Ai Quoc Sent: den 13 januari 2005 09:59 To: [log in to unmask] Subject: Re: [TN] Antw: [TN] Must we applied N2 to reflow when using Pb-free solder paste? Hi Guenter, Thanks so much for your advice. Actually, your idea is unique on this net about this topic. It seems nobody use no N2 for reflow. Best regards, England ----- Original Message ----- From: "Guenter Grossmann" <[log in to unmask]> To: <[log in to unmask]> Sent: Thursday, January 13, 2005 3:27 PM Subject: [TN] Antw: [TN] Must we applied N2 to reflow when using Pb-free solder paste? > John > > Reflow soldering Pb free is possible without N2. You will see some > problems with wetting. However, the reaction of the solder with the > metallisation takes place. I heard of rumors about reliability > problems when soldering without N2 but didn't read a paper so far. > > Best regards > > Guenter > > > > EMPA > Swiss Federal Laboratories for Materials Testing and Research Centre > for Reliability Guenter Grossmann, Senior Engineer > > 8600 Duebendorf > Switzerland > > Phone: xx41 1 823 4279 > Fax : xx41 1 823 4054 > mail: [log in to unmask] > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 1.8e To > unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt > or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: > http://listserv.ipc.org/archives Please visit IPC web site > http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 > ----------------------------------------------------- > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- - - - - - - - Appended by Scientific-Atlanta, Inc. - - - - - - - This e-mail and any attachments may contain information which is confidential, proprietary, privileged or otherwise protected by law. The information is solely intended for the named addressee (or a person responsible for delivering it to the addressee). If you are not the intended recipient of this message, you are not authorized to read, print, retain, copy or disseminate this message or any part of it. If you have received this e-mail in error, please notify the sender immediately by return e-mail and delete it from your computer. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------