Sorry, Doug, but it is more than the solvent/carrier system. With many fluxes, the activators themselves are VOCs and, if the residues sublimate, they are also VOCs. It is possible they may not be legally classed as VOCs in some countries, but that is a bureaucratic quibble, not science. In other countries, they are classed, by the definition that a VOC is an organic compound which is emitted into the air and which can photochemically react with NOxs to form the precursor compounds of tropospheric ozone. This is the case with many active flux components. I agree that the quantities emitted may be small compared with the solvent system, but they are not negligible. Brian Douglas O. Pauls wrote: > David, > VOCs are there as carrier solvents. Most liquid fluxes have a variety of > different VOCs in them of differing molecular weights so that they > volatilize at progressively later points in the reflow process. If your > reflow profile is optimized, they should all be gone well before the solder > liquidus point. If not, you can have problems. > > Doug Pauls > > > > > David Tremmel > <davidtremmel@HOT > MAIL.COM> To > Sent by: TechNet [log in to unmask] > <[log in to unmask]> cc > > Subject > 11/30/2004 02:50 [TN] VOCs > PM > > > Please respond to > TechNet E-Mail > Forum > <[log in to unmask]> > ; Please respond > to > David Tremmel > <davidtremmel@HOT > MAIL.COM> > > > > > > > Dear Technetters, > > VOCs (Volatile Organic Compounds) are part of many fluxes, but how do they > affect the wetting process, or do they burn off for the most part during > the > soldering process? > > TIA > > David > > _________________________________________________________________ > Visita MSN Latino Entretenimiento: ¡música, cine, chismes, TV y más...! > http://latino.msn.com/entretenimiento/ > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 > for additional information, or contact Keach Sasamori at [log in to unmask] or > 847-615-7100 ext.2815 > ----------------------------------------------------- > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 > ----------------------------------------------------- > > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------