Yes - I agree, the thickness range is set - 20-40. Jeffrey Bush Director, Quality Assurance and Technical Support VERMONT CIRCUITS INCORPORATED 76 Technology Drive - POB 1890 Brattleboro, Vermont 05302 Voice: 802.257.4571.21 Fax: 802.257.0011 http://www.vtcircuits.com -----Original Message----- From: R Sedlak [mailto:[log in to unmask]] Sent: Tuesday, November 30, 2004 6:31 PM To: [log in to unmask] Subject: Re: [TN] Immersion White Tin Plating Specification Before we go off writing specifcations that make the fabrications people spit and swear, I want to remind all that all immersion plating is self-limiting, and when all the substrate is covered, you stop plating, no matter what temperature, or how long you leave it in the plating bath... Most fabricators have trouble getting 50 microinches of Tin, and 40 is pretty much the standard... 30 is pretty considered pretty thin.. And, no flat finishes are going to perform as well as HASL, if only because of thickness, nevermind superiority of alloy... Rudy Sedlak RD Chemical Company --------------------------------- Do you Yahoo!? --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- All your favorites on one personal page - Try My Yahoo! --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------