The problem you have is too higher air flow, turn the air flow down and you will not blow the chips off the board. 0201 and even 01005 parts can be removed and the replaced with hot air. Bob Willis On 12/2/2004, "Le Ai Quoc" <[log in to unmask]> wrote: >Hi technetters, >Good morning! >Who among you here know how to use portable hot air rework method to repair >chip 0201 (0603mm). We use this equipment with non-flux solder wire. >We have some misalignment, tombstone at this chip and need to replace with >the new part. We had a portable hot air made by Hakko but to do this job, >actually it is very difficult. Normally, chip is blown away or solder wire >added to the electrode is too much. >What is the temperature profile for this chip? Because w/o profile, we don't >know the setting of temperature and hot air volume for this part when >reworked. >Thanks so much for your instruction, >Best regards, >Quoc > >--------------------------------------------------- >Technet Mail List provided as a service by IPC using LISTSERV 1.8e >To unsubscribe, send a message to [log in to unmask] with following text in >the BODY (NOT the subject field): SIGNOFF Technet >To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) >To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest >Search the archives of previous posts at: http://listserv.ipc.org/archives >Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 >----------------------------------------------------- > > > Bob Willis 2 Fourth Ave, Chelmsford Essex, CM1 4HA England Tel +44 01245 351502 Fax +44 01245 496123 Web www.leadfreesoldering.com --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------