i'd be inclined to talk to the faa and boeing about this since a 747 blew up over the atlantic because of a electical failure in the fuel tank. i mean PLEASE talk to the faa and boeing. -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Diamond, Pat Sent: Wednesday, December 08, 2004 5:04 AM To: [log in to unmask] Subject: [TN] Poor solder cup plating Hi Technetters, we have a potential problem, after our connector manufacturer went out of business, we tried an alternative approved company who manufactured some evaluation samples. The samples we received showed evidence of missing/contaminated plating in the bottom of the solder cups. After soldering and cross sectioning some of the cups, there was evidence of non-wetting and flux entrapment in the bottom of the cup. When we contacted our supplier, they stated that due to the configuration constraints and the plating method, they cannot guarantee to produce 100% plated parts every time (we have also had this confirmed by alternative sources). We have devised an alternative manufacturing method which will correct the problem but will not receive part for approximately 3 months! Some background information on the product: The unit the connectors are used on, is an aircraft fuel density sensor which sits in the fuel tank and measures the amount of fuel on board say a 747. After assembly, the connectors are potted with an epoxy and then electron beam welded to the sensor which has been previously evacuated to 3 E-4 Mbar. My question is; given that the solder has wetted fully on the outside (and most of the inside) of the cup and that the connectors are in a vacuum, will the flux entrapment cause corrosion etc. with the passage of time? A few bits of further info: * The cup is made from 1.02mm Diameter Nilo 50 and the plating is 2.5 microns of electro-tin, flow brightened over a copper undercoat * The solder used is HMP- 93.5%Pb/5% Sn/1.5%Ag * The flux used is Ersin 362 Rosin activated * The operating temperature spec is -55 +125 degrees C The other unfortunate problem is that we cannot change the cup material or the plating method! Any help/advice you can offer would be appreciated. Pat Diamond **************************************************************************** *************** The information transmitted is intended only for the person or entity to which it is addressed and may contain confidential and/or privileged material. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited. If you received this in error, please contact the sender and delete the material from any computer. **************************************************************************** *************** Pat Diamond Senior manufacturing Engineer Weston Aerospace Tel: +44 (0)1252 868122 124 Victoria Road Fax: +44 (0)1252 370298 Farnborough, Hampshire, GU14 7PW Web www.westonaero.com> England Email mailto:[log in to unmask] --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------