Just a note on Immersion White Tin, We have recently removed this finish from our fabrication spec and PCB drawings due to problems with the viscous chemistry being trapped in holes and causing opens after shipment to the customer. We have changed to Immersion Silver. Anyone had a similar experience? -Al Onderick -----Original Message----- From: [log in to unmask] [mailto:[log in to unmask]] On Behalf Of [log in to unmask] Sent: Tuesday, November 30, 2004 1:23 PM To: [log in to unmask] Subject: [TN] Immersion White Tin Plating Specification Hi Technet, Can anyone tell me what the plating specification (including thickness, etc.) should be for immersion white tin to be used for compliant pin (press-fit)? Also, is immersion white tin the preferred finish for press-fit, or is immersion silver or something else? Thank you in advance. Kaye Clayo Sr. P. C. Layout Designer Keithley Instruments, Inc. CONFIDENTIALITY NOTE: This message is intended only for the use of the individual or entity to which it is addressed and may contain information that is privileged, confidential, and exempt from disclosure under applicable law. If the reader of this notice is not the intended recipient, you are hereby notified that any dissemination, distribution or copying of this communication is strictly prohibited. If you have received this communication in error, please notify the sender immediately. __________________________________________________________________________ ___ Scanned by IBM Email Security Management Services powered by MessageLabs. For more information please visit http://www.ers.ibm.com __________________________________________________________________________ ___ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------