Steve, Thanks for the info. M Muthu Product Engineering Dept No. 99 Lebuhraya Kampung Jawa Taman Perindustrian 11900 bayan Lepas Penang, Malaysia Tel : 6420000 Fax: 6482222 -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Steve Sent: Wednesday, December 29, 2004 8:00 AM To: [log in to unmask] Subject: Re: [TN] 6 Mils STF Hi Muthu, As far as I am aware there are no manufacturer's of 6 mil polyimide. The best you can do is 5 mils with a mil of adhesive. It is made by DuPont only. Good luck. Steve Kelly --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------