Hole size requirements don't need to change for lead free solder. We have tested 6 different alloys now and all seem suitable for press fit pins. Happy to process test samples for anyone interested. -----Original Message----- From: Kaye Clayo [mailto:[log in to unmask]] Sent: Tuesday, November 30, 2004 9:25 PM To: [log in to unmask] Subject: Re: [TN] Immersion White Tin Plating Specification Jeffrey, I need to change the finish to comply with lead-free. Do you think that lead-free (SN100CL) HASL will work as well as SnPb HASL for press-fit connectors? It is probably too new to tell, huh? Can you tell me what the plating specification should be for white tin? Does 30-50uin sound correct? Is immersion white tin really called ISn or ImSn? Thanks again, Kaye At 04:02 PM 11/30/2004, you wrote: >With press-fit HASL is the best and with an alternate finish like ISN >or IAG the PTH size need to be re-evaluated for the new finish. > >Jeffrey Bush >Director, Quality Assurance and Technical Support > >VERMONT CIRCUITS INCORPORATED > 76 Technology Drive - POB 1890 > Brattleboro, Vermont 05302 > Voice: 802.257.4571.21 Fax: 802.257.0011 > http://www.vtcircuits.com > > >-----Original Message----- >From: Kaye Clayo [mailto:[log in to unmask]] >Sent: Tuesday, November 30, 2004 2:23 PM >To: [log in to unmask] >Subject: [TN] Immersion White Tin Plating Specification > >Hi Technet, > >Can anyone tell me what the plating specification (including thickness, >etc.) >should be for immersion white tin to be used for compliant pin >(press-fit)? > >Also, is immersion white tin the preferred finish for press-fit, or is >immersion silver or something else? > >Thank you in advance. > >Kaye Clayo >Sr. P. C. Layout Designer >Keithley Instruments, Inc. > >CONFIDENTIALITY NOTE: This message is intended only for the use of the >individual or entity to which it is addressed and may contain >information that is privileged, confidential, and exempt from >disclosure under applicable law. If the reader of this notice is not >the intended recipient, you are hereby notified that any dissemination, >distribution or copying of this communication is strictly prohibited. >If you have received this communication in error, please notify the >sender immediately. > > > >_______________________________________________________________________ >_ >_____ >Scanned by IBM Email Security Management Services powered by >MessageLabs. For more information please visit http://www.ers.ibm.com >________________________________________________________________________ >_____ > >--------------------------------------------------- >Technet Mail List provided as a service by IPC using LISTSERV 1.8e To >unsubscribe, send a message to [log in to unmask] with following text in >the BODY (NOT the subject field): SIGNOFF Technet >To temporarily halt or (re-start) delivery of Technet send e-mail to >[log in to unmask]: SET Technet NOMAIL or (MAIL) >To receive ONE mailing per day of all the posts: send e-mail to >[log in to unmask]: SET Technet Digest >Search the archives of previous posts at: >http://listserv.ipc.org/archives >Please visit IPC web site >http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional >information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 >ext.2815 >----------------------------------------------------- > > >_______________________________________________________________________ >______ >Scanned by IBM Email Security Management Services powered by MessageLabs. For more information please visit http://www.ers.ibm.com >___________________________________________________________________________ __ CONFIDENTIALITY NOTE: This message is intended only for the use of the individual or entity to which it is addressed and may contain information that is privileged, confidential, and exempt from disclosure under applicable law. If the reader of this notice is not the intended recipient, you are hereby notified that any dissemination, distribution or copying of this communication is strictly prohibited. If you have received this communication in error, please notify the sender immediately. ____________________________________________________________________________ _ Scanned by IBM Email Security Management Services powered by MessageLabs. For more information please visit http://www.ers.ibm.com ____________________________________________________________________________ _ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------