Yea.. but whose counting? LOL It started out to be one question... but as I typed it I had more.. I should have gone back to update the count there... but yea... its Friday... almost lunch time... :) So it sounds like Immersion Silver has the best of all worlds with the one caveat in the presence of sulpher it can be nasty... but even then... can't the board be stripped and replated to recover it? Is that costly? I really see no downside to silver immersion then... unless there is something that hasn't been covered... compatibility with all processes, not even ionic contamination issues in the washing process... no issues?... I like it. I may have a talk with our MFG ENG and see what he thinks of switching from ENIG to IAg. For our fine pitch parts. Getting the nickel out of the process is probably a good thing...for RF. What about cost vs. IAg? Best regards, Bill Brooks - KG6VVP PCB Design Engineer , C.I.D.+, C.I.I. Tel: (760)597-1500 Ext 3772 Fax: (760)597-1510 e-mail:[log in to unmask] http://www.dtwc.com http://pcbwizards.com -----Original Message----- From: Wenger, George M. [mailto:[log in to unmask]] Sent: Friday, December 03, 2004 11:29 AM To: TechNet E-Mail Forum; Brooks,Bill Subject: RE: [TN] HAL Finish Bill, It is Friday and I had a rough week. I missed the fact that you actually asked 6 questions. 5. Yes but not significantly. 6. Yes it will but if the Pb-Free is SAC you'll not be able to measure the small amount of Ag contamination. Regards, George George M. Wenger (908)-546-4531 Reliability / FMA Engineer Base Station and Subsystems Group Andrew Corporation, 40 Technology Drive, Warren, NJ 07059 [log in to unmask] -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Wenger, George M. Sent: Friday, December 03, 2004 2:09 PM To: [log in to unmask] Subject: Re: [TN] HAL Finish Bill, You start out saying "One question I would have regarding Immersion Silver" and then you ask 4 questions. here are my answers to the 4 questions. 1.nothing 2. Nothing significant 3. No 4. No Regards, George George M. Wenger (908)-546-4531 Reliability / FMA Engineer Base Station and Subsystems Group Andrew Corporation, 40 Technology Drive, Warren, NJ 07059 [log in to unmask] -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Brooks,Bill Sent: Friday, December 03, 2004 1:55 PM To: [log in to unmask] Subject: Re: [TN] HAL Finish One question I would have regarding Immersion Silver. What does it do to the solder metallurgically? Anything at all? Do they require an under plating barrier for immersion silver like they do with the nickel/gold immersion gold process? Is there a silver dendrite issue? If you were using a wave solder process with surface mount would the silver contaminate the bath over time? What about lead free wave solder? There are so many things that affect the decision to go with a process that are not just joint quality related... The world keeps turning and the only constant is change itself... Best regards, Bill Brooks - KG6VVP PCB Design Engineer , C.I.D.+, C.I.I. Tel: (760)597-1500 Ext 3772 Fax: (760)597-1510 e-mail:[log in to unmask] http://www.dtwc.com http://pcbwizards.com -----Original Message----- From: Roger Stoops [mailto:[log in to unmask]] Sent: Friday, December 03, 2004 10:30 AM To: [log in to unmask] Subject: Re: [TN] HAL Finish Their email just said they wanted lead-free HAL, no IAg. Then they said "...Immersion Silver is not suitable for long storage which is leading to other problems." Like Lee said, bizarre! What is long-storage? Anything over 6-12 months is not good anyway for lean/JIT manufacturing, or so I thought. Got some boards from a reputable fab house with IAg plating just this week, and they were packaged to last a long time: sulfur-free paper between each board, 10 boards per well-sealed shrink wrap plastic pack with desiccant inside pack. Sounds like they have their act together, no? But sometimes we are required to use certain vendors, and I have to make my designs compatible with each one...and not necessarily all at the same time. BRgds, Roger Like Courage says, "What I do for love..." -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Wenger, George M. Sent: Friday, December 03, 2004 12:12 PM To: [log in to unmask] Subject: Re: [TN] HAL Finish Did your EMS vendor give you any reasons why they will not accept boards with IAg plating. It tould be good to know if they have documentation of a problem or if they simply have a fear. Regards, George George M. Wenger (908)-546-4531 Reliability / FMA Engineer Base Station and Subsystems Group Andrew Corporation, 40 Technology Drive, Warren, NJ 07059 [log in to unmask] -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Roger Stoops Sent: Friday, December 03, 2004 12:08 PM To: [log in to unmask] Subject: [TN] HAL Finish One of our EMS vendors has told us they will not accept boards with IAg plating. Instead, they want HAL, which I assume they want hot-air leveled Sn. Any pros and cons anyone would like to share from the board fab, assembly and test viewpoints? Any advantage to plating Sn over Ni, or just a waste of money/not necessary? Many thanks in advance, Roger --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ---------------------------------------------------------------------------- -------------------- This message is for the designated recipient only and may contain privileged, proprietary, or otherwise private information. If you have received it in error, please notify the sender immediately and delete the original. Any unauthorized use of this email is prohibited. ---------------------------------------------------------------------------- -------------------- [mf2] --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ---------------------------------------------------------------------------- -------------------- This message is for the designated recipient only and may contain privileged, proprietary, or otherwise private information. If you have received it in error, please notify the sender immediately and delete the original. Any unauthorized use of this email is prohibited. ---------------------------------------------------------------------------- -------------------- [mf2] --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ---------------------------------------------------------------------------- -------------------- This message is for the designated recipient only and may contain privileged, proprietary, or otherwise private information. If you have received it in error, please notify the sender immediately and delete the original. Any unauthorized use of this email is prohibited. ---------------------------------------------------------------------------- -------------------- [mf2] --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------