Ted, You will need to contact your PWB supplier because the coupons must come from the fab house that you use. They must also be from the same substrate configuration (i.e. material, soldermask and surface finish) that you use. If you are going to comply with IPC requirements you will need coupons from each supplier and each fab configuration that you have. Therefore, you cannot simply purchase off the shelf coupons. Sorry. Perhaps your fab house will have some with your configuration already available. Russell Nowland Lucent Technologies Quail Springs Parkway Plaza 14000 Quail Springs Parkway. Suite 300 Oklahoma City, OK 73134 Phone: 405-302-1660 Fax: 405-302-1622 Cell: 405-203-0034 email: [log in to unmask] -----Original Message----- From: Ted Kong [mailto:[log in to unmask]] Sent: Monday, December 13, 2004 7:59 PM To: [log in to unmask] Subject: [TN] SIR coupons and test Hi Fellow Technetter, Does anyone know a place to get off-the-shelf SIR test coupons. IPC supposes to have it, but nothing showed up when I search for "B-24". I am also looking for a place that can run the SIR test as well. Please let me know it anyone out there has a contact. Thanks all in advance. Ted __________________________________ Do you Yahoo!? Yahoo! Mail - 250MB free storage. Do more. Manage less. http://info.mail.yahoo.com/mail_250 --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------