I agree wholeheartedly. I attended a seminar yesterday at Villanova University where Jim McElroy of NEMI, Karl Seelig of AIM, Dennis Barbini of Vitronics Soltec and Jack Geibig of the Center for Clean Products and Clean Technologies at the University of Tennessee were presenters. The primary take-aways were: 1. It is going to cost everyone more to manufacture lead-free products, due to more expensive solder, higher energy requirements in processes, etc. 2. The reliability of lead-free solders and connections made with these solders has not been proven. And the most interesting part was that the study conducted by U of Tenn showed that the use of SAC solders causes more harm to the environment than the use of SnPb. The UT website relating to this is at: http://eerc.ra.utk.edu/ccpct/lfsp-projectinfo.html however, the results of the study are not yet available there. Blair >>> [log in to unmask] 11/19/04 12:36PM >>> Good artlicle. A beginning of a movement in the right direction? ******************************************************************* This email and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this email in error please notify the system manager. This footnote also confirms that this email message has been swept for the presence of computer viruses. www.hubbell.com - Hubbell Incorporated --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------