Scot - take a look at the draft document 4553 - I Ag specification. We are saying in that document that I Ag will have 12 months shelf life. Solderability is excellent for I Ag and based on our costs at Photocircuits Corporation it is most definitely less expensive than ENIG. We are in the process of finalizing the technical paper to justify this specification. In it I tested five different I Ag suppliers in real time without protecting the finish. After day 763, the I Ag test strip if covered by another test strip produces positive wetting, wetting times under 2 seconds and does not show any signs of dewetting, if the test strip was unprotected then it fails, only to be expected, but after 763 DAYS!. Regards Gerard O'Brien Co-chairman 4-14 plating committee Photocircuits Corporation -----Original Message----- From: Scott Lefebvre [mailto:[log in to unmask]] Sent: Wednesday, November 24, 2004 1:43 PM To: [log in to unmask] Subject: [TN] Immersion Silver I just got off the phone with one of our PCB FAB shops and was surprised on his response to Immersion Silver as a solder finish. He suggested that we do not use it as a replacement for HASL and to use gold instead. All the things I've read and did research on IAg in contraction to he said. The shop said shelf life is less than 6 months and tarnish was a big issue. It was more expensive than ENIG and not that many shops do it in-house. My understanding is the shelf life is 6-12 months if stored and handled properly. They silver used today has an anti-tarnishing agents to prevent tarnishing. I was also under the impression that IAg is less costly than ENIG. Your opinion in this matter would be greatly appreciated. Thank you, Scott --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------