I've noticed similar 'goo' with repairs I have done on TV / VCR remotes. I always use IPA. However, the outer touch surface of the elastomer pads usually show a brown 'goo' on the wipe or swab after cleaning, and the internal surfaces leave a black 'goo' on the wipe or swab. I'm thinking the elastomer pads are printed with a carbon ink to make the connection when pressed against the interleaved 'pitch fork' pads on the board. The plated pads on the board usually leave a brown 'goo' on the wipe or swab. After a thorough cleaning, I usually leave the pieces on a paper towel for a couple of hours to dry, then reassemble the components. I've even performed this routine on a remote that was dropped into a fish tank! Still works good to this day! I have also noticed that repairs done on units that reside in smokers dwellings reveal a darker brown 'goo'. I've never noticed any type of sealing compound, such as dielectric silicone grease or glue on hand held units taken apart for repair. If you have access to one, a SEM should reveal the chemistry behind the brown 'goo' phenomenon. Or maybe you could send a 'goo' sample to your local CSI lab to see if there is any DNA within it. ??? My favorite tool is the Victorinox 'Swiss Champ', don't know what I would do without it, except carry around a small tool box! Dave Simonik Sanmina-SCI Owego NY Division -----Original Message----- From: Blair K. Hogg [mailto:[log in to unmask]] Sent: Friday, November 05, 2004 9:42 AM To: [log in to unmask] Subject: A Friday question Greetings 'netters: Had the occasion last night to perform surgery on a cordless telephone, the buttons had become dysfunctional rendering the phone basically unusable. I've done this on other phones before, and each time have found that the elastomer switch panel and printed circuit board have become coated with some kind of "goo". I believe that this "goo" is the accumulation of skin oils which somehow migrate into the phone and get under the elastomer, but have thought that perhaps some manufacturers intentionally put some kind of compound on the elastomer for some reason (sealing?). I'm leaning toward the skin oil explanation, since we make products here with elastomer switch panels and have never used any sealing compound during assembly. Anyone else out there doing this kind of assembly and do you put anything on the elastomer during assembly? Also, in the past I've cleaned up the elastomer with drug store IPA (91%), but here I was last night working in the kitchen with a Swiss army knife (one with all the tools on it) and there next to me was the sink and a bottle of Palmolive detergent. Well, I though, aqueous wash, and went at it. It worked pretty well, but after reassembly the left over moisture began condensing on the window and it was hard to see the display. I'm sure this will clear up after a while, though. So what do you cleaning gurus think is the best way to remove the "goo", whatever it is? IPA or Palmolive? Is Palmolive a saponifier or a surfactant, or both? Happy Friday, Blair ******************************************************************* This email and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this email in error please notify the system manager. This footnote also confirms that this email message has been swept for the presence of computer viruses. www.hubbell.com - Hubbell Incorporated --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ____________________________________________________________________________ _ Scanned by Sanmina-SCI eShield ____________________________________________________________________________ _ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------